Common problems and solutions in the production of fiberglass tubing

Release time:

2025-03-12 10:41

一、Why do fiberglass tubes have stains

The smoothness, cleanliness, and tidiness of the surface produced by fiberglass tubes are the basis for ensuring their appearance. Occasionally, stains, especially black oil stains, are found on fiberglass pipes during production.

What are the reasons for the stains on fiberglass pipes?

1. Caused by the previous process

2. Water stains, oil stains, or other contaminants on the billet tube at the pass through point

3. Cross color

4. Dragging the floor contaminated with dust or other debris

5. The paint is not clean, there are impurities or mixed with other colors

6. How to reduce the occurrence of stains on fiberglass tubes? Firstly, it is important to regularly clean and maintain the equipment. With a relatively complete process flow, 5S cleaning work should be done well. Secondly, strengthen the quality inspection work of the quality department to avoid the outflow of defective products

 

二、What causes uneven color of fiberglass tubes

The production process of fiberglass tubes is relatively simple, with several main steps including weaving, painting and gluing, packaging and warehousing. Why does this process lead to uneven color of fiberglass tubes? Let's analyze it with our regular white fiberglass tubes.

The reasons for uneven color of fiberglass tubes are as follows:

1. Inappropriate setting of dewaxing temperature

2. Unstable dewaxing temperature

3. External cold air enters the dewaxing furnace

4. Abnormal weaving of billet tube

 

三、Reasons for insufficient (stable) voltage resistance of fiberglass tubing

Fiberglass tubes can be divided into 1.2kV fiberglass tubes, 1.5kV fiberglass tubes, 2.5kV fiberglass tubes, 4kV fiberglass tubes, and 7kV fiberglass sleeves according to their voltage resistance levels. Among them, 1.2kV fiberglass tubes and 1.5kV fiberglass tubes have been unified into 1.5kV fiberglass sleeves due to their similar processes and voltage resistance levels.

According to technical standards, the actual withstand voltage level of fiberglass sleeves during production should be much higher than the nominal voltage value. For example, the withstand voltage of 1.5kV fiberglass tubes can reach around 2.5KV. In industry standards, fiberglass tubes may occasionally have some extreme individual values, such as the actual withstand voltage value of 1kV measured at a certain node for fiberglass tubes with a withstand voltage of 1.5kV. This is allowed in industry standards and may not necessarily be unqualified products.

 

What are the reasons for the insufficient (stable) voltage resistance level of fiberglass tubing when it is detected to be unqualified?

1. Low paint concentration

2. Bubble formation

3. Raw rubber quality issues

4. Poor weaving of the billet tube, too sparse and loose

5. Employee operation error

 

 

 

 

Dongguan Keyu New Material Technology Co., Ltd. welcomes customers to inquire: