YST/H-High Shrink Polyester Heat Shrink Tubing ( Thermal Polyester Sleeving)
Product Overview:
- Product Features
- Specifications
- Technical data
- Video
-
KEYUACE 's Polyester Film Heat Shrink Tubing produced by is made of PET polyester film spirally wound and bonded with special glue. This glue is composed of a unique epoxy resin and has chemical similarity and compatibility with PET polyester film.
YST-H -High-ratio polyester thermal shrink Sleeving has been proven to have extremely reliable insulation performance, ultra-thin wall thickness, high dielectric properties and continuous operation at 150°C.
Polyester film can be used in combination with plastic film, paper and other materials, and spirally wound. Therefore, when you need a composite tubing.
YST-H -Polyester PET Film Tubing is available in no-shrink, low-shrink and high-shrink materials.
Application:
High-ratio polyester heat shrink tubing is often used for insulation protection in the compressor and motor fields.
Typical Applications Include electric motors, thermal sensors, capacitor covers, battery sleeving EV motor slot insulation, medical tubing and countless others.
This series of products meets ROHS and REACH tests and meets environmental protection requirements.
-
YST-H - High-ratio heat shrink tubing for compressors (also called polyester thermal shrink shrink sleeves).
Specification
Inner Diameter
ID1.2 ~ ID79.1mm
Can be customized according to customer needsInner diameter tolerance
Can be customized according to customer needs
Thickness
0.025~1.0mm
Can be customized according to customer needsThickness tolerance
Can be customized according to customer needs
Lenght
1000mm
Can be customized according to customer needsLength Tolerance
Can be customized according to customer needs
We can supply transparent sleeves, sleeves with stripes in various colors, sleeves with printing, patterns, etc.
-
Performance Parameters
Features
Date
Test Method
Melting point
250~255℃
——
Operating temperature
-60 ℃ ~150℃
——
Breakdown voltage
1KV/1 minute, No breakdown
ASTMD149
Thermal shrinkage (raw material)
25%-50%
——
If custo mers require more detailed information on dimensional tolerances or printing, please consult our sales department.